Fresae Extremae Longitudinis Standardis Duarum Canalium Carbide HRC55
Materia Rudis: Utere ZK30UF cum 12% Co contento et 0.6um granorum magnitudine.
Tegumentum: AlTiSiN, cum duritia et stabilitate thermali usque ad 4000HV et 1200℃ respective.
Tolerantia Diametri Fresae Extremae: 1 < D≤6 -0.010 ~ -0.030; 6 < D≤10 -0.015 ~ -0.040; 10 < D≤20 -0.020 ~ -0.050
Tegumentum: AlTiSiN, magna copia aluminii praebet duritiem calidam excellentem et resistentiam oxidationis.
Fluctus: Duo fluctus, apti ad ablationem fragmentorum, facile ad processum verticaliter alimentorum, late in processu fissurarum et foraminum adhibiti.
Tolerantia Diametri Fresae Extremae:
1 < D ≤ 6 -0.010 ~ -0.030
6 < D ≤ 10 -0.015 ~ -0.040
10 < D ≤ 20 -0.020 ~ -0.050
Parametri Secandi:
Vc = 220 (100-800) m/min
ap=1/2D(1/8-3/4D)
ae = 1/2D(1/4 - 1D)
fz = 0.15mm (0.02-0.2)
Angulus spiralis est 35 graduum, qui fortem adaptabilitatem ad materiam et ha habet.
Specificatio:
| Numerus item | Diameter D | Longitudo Secandi | Diametros Caniculi | Longitudo Totalis | Tibiae |
| MSKEM4FD001 | 3 | 8 | 3 | 50 | 2 |
| MSKEM4FD002 | 1 | 3 | 4 | 50 | 2 |
| MSKEM4FD003 | 1.5 | 4 | 4 | 50 | 2 |
| MSKEM4FD004 | 2 | 6 | 4 | 50 | 2 |
| MSKEM4FD005 | 2.5 | 7 | 4 | 50 | 2 |
| MSKEM4FD006 | 3 | 8 | 4 | 50 | 2 |
| MSKEM4FD007 | 4 | 10 | 4 | 50 | 2 |
| MSKEM4FD008 | 5 | 13 | 5 | 50 | 2 |
| MSKEM4FD009 | 5 | 13 | 6 | 50 | 2 |
| MSKEM4FD010 | 6 | 15 | 6 | 50 | 2 |
| MSKEM4FD011 | 7 | 18 | 8 | 60 | 2 |
| MSKEM4FD012 | 8 | 20 | 8 | 60 | 2 |
| MSKEM4FD013 | 10 | 25 | 10 | 75 | 2 |
| MSKEM4FD014 | 12 | 30 | 12 | 75 | 2 |
| MSKEM4FD015 | 14 | 35 | 14 | 80 | 2 |
| MSKEM4FD016 | 14 | 45 | 14 | centum | 2 |
| MSKEM4FD017 | 16 | 45 | 16 | centum | 2 |
| MSKEM4FD018 | 18 | 45 | 18 | centum | 2 |
| MSKEM4FD019 | 20 | 45 | 20 | centum | 2 |
| Materia Operis | ||||||
| Chalybs Carbonicus | Chalybs Mixtus | Ferrum Fusum | Mixtura Aluminii | Mixtura Cuprea | Chalybs Inoxidabilis | Chalybs Duratus |
| Idoneus | Idoneus | Idoneus | Idoneus | Idoneus | ||